LOSS OF ADHESION TO PLASTICS

Flaking coating as a result of loss of adhesion to plastics.

Causes
  • insufficiently cleaned substrate before coating,
  • not used adhesion increasing agent.
Prevention
  • heat the object to be coated sufficiently before cleaning,
  • clean thoroughly,
  • apply the adhesion increasing agent.
Repair
Sand and apply coat again.
 