HOLOGRAM EFFECT AFTER POLISHING

Polishing traces with reduced gloss.

Causes
  • too short drying time,
  • too much thickness across the coating,
  • wrong amount of hardener
  • too strong buffer pressure on varnished surface,
  • tilting side to side while operating the buffer,
  • applying wrong buffing compound,
  • polishing at too high a temperature.
Prevention
  • compliance with recommended thickness of coat layers, drying times and quantities of hardener
  • apply appropriate materials and tools for buffing in accordance with the technology used.
Repair
Dry the applied basecoat and apply it again.
 